Typical Tensile Properties
As welded | ||
Elongation | Tensile Strength | Yield Strength |
28 % | 556 MPa | 490 MPa |
Typical Charpy V-Notch Properties
As welded | |
Impact Value | Testing Temperature |
100 J | -20 °C |
– | -29 °C |
Typical Weld Metal Analysis %
Mn | C | Si |
1.36 % | 0.05 % | 0.45 % |
Deposition Data
Diameter | Current | Deposition Rate | Voltage | Wire Feed Speed |
1.4 mm | 250-370 A | 3,5-5,8 kg/h | 27-37 V | 7,1-11,8 m/min |
1.2 mm | 250-310 A | 4,2-5,8 kg/h | 27-33 V | 11,5-15,9 m/min |
1.6 mm | 250-370 A | 3,1-5,4 kg/h | 27-36 V | 4,8-8,9 m/min |
Approvals: | ABS, 3YSA H10, BKI, 3YH10SM, BV, S3YM H10, CCS, 3YSH10, CE, EN 13479, CWB, CSA W48-06 E491T-1-H8, DNV, III YMS (H10), GL, 3YH10S, LR, 3YS H10, NAKS/HAKC, 1.2MM, RS, 3Y40MS H10 |
Classifications: | SFA/AWS A5.36, E71T1-C1A2-CS1-H8, Weld Metal, JIS Z 3313, T49J0T1-1CA-U, Weld Metal, EN ISO 17632-A, T 46 2 P C1 1 H10, Weld Metal |
Approvals are based on factory location. Please contact ESAB for more information.
Alloy Type: | C Mn |
Welding Current: | DC+ |