Typical Tensile Properties
| ISO As welded | ||
| Elongation | Tensile Strength | Yield Strength |
| 32 % | 610 MPa | 510 MPa |
| AWS As welded | ||
| Elongation | Tensile Strength | Yield Strength |
| – | – | – |
Typical Charpy V-Notch Properties
| ISO As welded | |
| Impact Value | Testing Temperature |
| 50 J | 20 °C |
| 35 J | -20 °C |
Typical Weld Metal Analysis %
| Mn | Mo | C | Si | Ferrite FN | Ni | N | Cr |
| 0.6 % | 2.8 % | 0.02 % | 0.8 % | 18 % | 13.4 % | 0.09 % | 22.5 % |
Deposition Data
| Diameter | Current | Deposition Rate | Fusion time per electrode at 90% I max | kg weld metal/kg electrodes | Number of electrodes/kg weld metal | Voltage |
| 2.5 x 300 mm | 50-90 A | 0.9 kg/h | 45 sec | 0.57 kg | 94 | 29 V |
| 4.0 x 350 mm | 85-180 A | 2.0 kg/h | 56 sec | 0.61 kg | 32 | 31 V |
| 3.2 x 350 mm | 60-120 A | 1.4 kg/h | 61 sec | 0.59 kg | 47 | 27 V |
| 5.0 x 350 mm | 110-250 A | 2.7 kg/h | 64 sec | 0.59 kg | 20 | 30 V |
| 2.0 x 300 mm | 40-60 A | 0.6 kg/h | 48 sec | 0.58 kg | 147 | 26 V |
| Approvals: | ABS, SS to C&C/Mn steels, BV, 309Mo, CE, EN 13479, CWB, CSA W48: E309LMo-17, DB, 30.039.05, DNV-GL, VL 309 Mo, LR, SS/CMn, RINA, 309Mo, Seproz, UNA 272580, VdTÜV, 02424 |
| Classifications: | EN ISO 3581-A, E 23 12 2 L R 3 2, SFA/AWS A5.4, E309LMo-17, CSA W48, E309LMo-17, Werkstoffnummer, 1.4459 |
Approvals are based on factory location. Please contact ESAB for more information.
| Alloy Type: | Austenitic CrNi |
| Coating Type: | Acid Rutile |
| Ferrite Content: | FN 12-22 |
| Welding Current: | DC+, AC |